Designation |
|
Description and applications
|
|
|
|
|
Tubular composite electrode, designed for high deposition rate welding of carbon-manganese steels. Can be used for single and multi-pass welding. |
|
|
|
|
Nickel alloyed, tubular composite electrode, producing excellent metal toughness down to -50°C. The high deposition rate and excellent mechanical properties make this wire an ideal choice for many off-shore applications. |
|
|
|
|
Nickel alloyed, tubular composite electrode, producing excellent metal toughness down to -60°C. The high deposition rate and excellent mechanical properties make this wire an ideal choice for many offshore applications. |
|
|
|
|
Tubular composite electrode alloyed with 0.5 % molybdenum. Designed for high deposition rate welding of higher strength steels. |
|
|
|
|
1.25% chromium and 0.5% molybdenum alloyed tubular composite electrode, designed for high deposition rate submerged-arc welding of heat resisting steels of similar composition. |
|
|
|
|
2.5% chromium and 1% molybdenum alloyed tubular composite electrode, designed for high deposition rate submerged-arc welding of heat resisting steels of similar composition. |
|
|
|
|
Tubular composite electrode, designed for high deposition rate submerged-arc welding of weathering steels. |
|
|
|
|
Nickel chromium molybdenum tubular composite electrode, designed for high deposition rate submerged-arc welding of low alloyed , fine-grained, high tensile strength steels. |
|
|
|
|
Nickel chromium molybdenum tubular composite electrode, designed for high deposition rate submerged-arc welding of low alloyed , fine-grained, high tensile strength steels. |